APS-1A
It used for the manufacture teploprochnogo deformable material such as SAP
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Aluminum Lumpy Powder |
Chemical composition
| Standard | Fe, % | Al, % |
|---|---|---|
| GOST 10096-76 | < 0.2 | > 99.8 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10096-76 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Al | % | Aluminium |