AT-6
for the production of cavitation-resistant products; class structure of α + β
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Titanium, titanium alloys |
Wrought Titanium Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Cr, % |
Ti, % |
Al, % |
|
1.5–1.5 |
1.5–1.5 |
1.5–1.5 |
89.9–91.4 |
5–6.5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\psi$$, % |
Treatment |
| Forgings |
|
|
|
|
1000–1100 |
10–15 |
25–40 |
|
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Al |
% |
Aluminium |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\psi$$ |
% |
Reduction in cross section on fracture |