АВ 87
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Deoxidation aluminum |
Chemical composition
| Standard | Si, % | Sn, % | Mg, % | Cu, % | Zn, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|
| GOST 295-98 | < 5 | < 0.2 | < 3 | < 3.8 | < 3.3 | > 87 | < 0.3 | < 13 |
Note: Al + Mg > 87.0
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 295-98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |