AV86
Aluminum is made in the form of pigs and pellets. The pigs are manufactured with a mass of not more than 20 kg, as well as small-sized pigs with a mass of not more than 4 kg.
For deoxidation, manufacture of ferroalloys and aluminothermy
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Deoxidation aluminum |
Chemical composition
| Standard | Si, % | Sn, % | Mg, % | Cu, % | Zn, % | Pb, % | Al + Mg, % |
|---|---|---|---|---|---|---|---|
| GOST 295-98 | < 5 | < 0.2 | < 3 | < 4 | < 3.5 | < 0.3 | < 86 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 295-98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Pb | % | Lead |
| Al + Mg | % | Aluminium + Magnesium |