AVD1
For the manufacture of ingots, processed by pressure, as well as for blending in the manufacture of aluminum alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1131-76 | < 0.8 | < 0.8 | 0.1–1 | 0.1–1 | 2.5–5 | < 0.5 | < 0.1 | 90.8–97.3 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1131-76 | GOST 1131-76 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |