ABE
For the manufacture of wire rod, obtained by continuous casting and rolling, and intended for the manufacture of wire for electrical purposes.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | V, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 20967-75 | 0.4–0.7 | 0.45–0.6 | 0.45–0.6 | < 0.00375 | < 0.00375 | < 0.00375 | < 0.05 | < 0.05 | < 0.00375 | 97.985–98.7 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Wire | GOST 20967-75 | 118–132 |
Standards
| Standard | Description |
|---|---|
| GOST 20967-75 | GOST 20967 - 75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| V | % | Vanadium |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |