AZh0.6
Aluminium foil for packaging.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Technical aluminum |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|---|
| GOST 745-2003 | 0.4–0.6 | < 0.2 | < 0.03 | < 0.01 | < 0.06 | 99–99.2 | < 0.4 | < 0.03 |