AZH-1
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Primary aluminum |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|
| 0.95–1.15 | < 0.2 | < 0.03 | < 0.01 | < 0.06 | 98.35–98.55 | < 0.05 | < 0.5 |