AZH1
For the manufacture of cold-rolled foil, designed for packaging of foodstuffs, medical products.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|
| GOST 745-2003 | 0.95–1.15 | < 0.2 | < 0.03 | < 0.01 | < 0.06 | 98.55–99.05 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 2710 |
Standards
| Standard | Description |
|---|---|
| GOST 745-2003 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |