B 133 (C 10400)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper |
Chemical composition
| Standard | Cu, % | Ag, % | O, % |
|---|---|---|---|
| ASTM B133 | > 99.95 | > 0.027 | < 0.001 |
Note: Cu: Cu + Ag
Information on suppliers
Analogues
| Germany | European Union | USA | Russia |
|---|---|---|---|
| OF-Cu DIN 1708 | Cu-OF EN 12165:2011 | OF | М0б Включен в 3 стандарта |
Standards
| Standard | Description |
|---|---|
| ASTM B133 | B 133 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Cu | % | Copper |
| Ag | % | Silver |
| O | % | Oxygen |