BN
babbits for manufacturing ingots used to fill the bearings and other parts; pouring temperature of 480−500 ° C; melting onset temperature of 240 ° C. Bearings operating at moderate speeds and medium loads; load characteristics — quiet shock.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tin, lead, babity |
lead babbit |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
Cd, % |
| GOST 1320-74 |
< 0.1 |
9–11 |
< 0.1 |
1.5–2 |
< 0.02 |
0.1–0.5 |
13–15 |
< 0.05 |
69.63–75.8 |
0.5–0.9 |
0.1–0.7 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
9550 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
Treatment |
| Alloy |
GOST 1320-74 |
|
|
|
125–130 |
70–74 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
GOST 1320-74 |
|
270–290 |
Casting and technological parameters
| melting point, °C |
temperature fill, °C |
| 400 |
480–500 |
Limit operating modes
| Standard |
Нагрузка, $$\textit{MPa}$$ |
Скорость, $$\frac{m}{s}$$ |
Температура, °C |
| GOST 1320-74 |
10 |
30 |
70 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| Cd |
% |
Cadmium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| temperature fill |
°C |
The temperature at which the fill metal in the form |