Br AZh9-4L
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
P, % |
Примеси, % |
| OST 24.916.01 |
2–4 |
< 0.2 |
< 0.2 |
< 0.5 |
80.1–90 |
< 1 |
< 1 |
< 0.05 |
8–10 |
< 0.1 |
< 0.05 |
< 0.1 |
< 2.7 |
Information on suppliers
Analogues
| Germany |
USA |
| 2.1816 |
80-10-10 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |