Br OFN 10-0.7-0.5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
P, % |
S, % |
Примеси, % |
| OST 24.916.01 |
< 0.2 |
< 0.2 |
8–12 |
83.9–91.2 |
< 0.35 |
0.4–1 |
< 0.25 |
< 0.35 |
0.4–0.7 |
< 0.05 |
< 1 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |
| S |
% |
Sulfur |