Br OTsN 10-2-1,5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
S, % |
Примеси, % |
| OST 24.916.01 |
< 0.3 |
< 0.02 |
9–11 |
< 0.005 |
81.605–89 |
1–3 |
1–2 |
< 0.5 |
< 0.02 |
< 0.5 |
< 0.05 |
< 1 |