BrA7Zh1.5S1.5
for casting of simple shape, heavy duty
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Tinless cast bronze |
Chemical composition
| Standard | Fe, % | Cu, % | Al, % | Pb, % |
|---|---|---|---|---|
| 1–1.5 | 87.5–92 | 6–8 | 1–1.5 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| GOST 2685-75 |