BrAZhNmts8.5-4-5-1.5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Sn, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
V, % |
Al, % |
Pb, % |
P, % |
C, % |
Примеси, % |
| TU 48-0820-300-84 |
3.7–4.3 |
< 0.1 |
0.005–0.01 |
< 0.1 |
1–1.8 |
76.87–82.39 |
< 1 |
4.7–5.3 |
0.005–0.01 |
8.2–9 |
< 0.01 |
< 0.05 |
< 0.05 |
< 1.4 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |
| C |
% |
Carbon |