BrHT0.6-0.5 (BrX0.6T0.5)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Cr, % | Ti, % | Cu, % |
|---|---|---|---|
| TU 48-21-283-73 | < 0.6 | < 0.5 | > 98.9 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 48-21-283-73 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |