BrMg0.8
Application: slip rings, collector plates, wires, cables
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Bronze, heatproof |
Chemical composition
| Standard | Fe, % | Mg, % | Cu, % |
|---|---|---|---|
| GOST 614-97 | < 0.05 | 0.7–1 | 98.9–99.3 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | δ, % | Treatment |
|---|---|---|---|---|---|---|---|
| Wire | GOST 614-97 | 250 | 30 |