BrNHK
Temperature hot processing 750−950 degrees Celsius.
Rings of pipe-welding machines, electrodes, heat exchangers, crystallizers, fasteners, tools
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Bronze, heatproof |
Information on suppliers
Physical characteristics
| Temperature, °C | $$E\cdot 10^{9}$$, $$MPa$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|---|---|
| 20 | 1.4 | 196 | 8850 | 37.2 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|
| Round | GOST 614-97 | 800 | 780 | 50 | 10 |
Standards
| Standard | Description |
|---|---|
| GOST 614-97 |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$E\cdot 10^{9}$$ | $$MPa$$ | Elastic modulus |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\psi$$ | % | Reduction in cross section on fracture |