BrO3.5Ts7S5
for the production of castings of valves General purpose; details of pipe fittings; antifriction parts
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Tin cast bronze |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
8700 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{0.5}$$, $$MPa$$ |
Treatment |
| Casting |
|
|
|
in sandy form |
145 |
6 |
|
| Casting |
|
|
|
in chill mold |
175 |
4 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
|
59 |
Standards
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{0.5}$$ |
$$MPa$$ |
Tensile stress required to produce a total elongation of 0.5% |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |