Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Tin cast bronze |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Cu, % |
Zn, % |
Sb, % |
Al, % |
Pb, % |
P, % |
| GOST 613-79 |
< 0.4 |
< 0.02 |
2–3.5 |
74.2–87 |
8–15 |
< 0.5 |
< 0.02 |
3–6 |
< 0.05 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
82.3 |
8700 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Round |
|
|
|
|
180–220 |
16–20 |
|
| Casting |
GOST 613-79 |
|
|
in chill mold |
206 |
5 |
|
| Casting |
GOST 613-79 |
|
|
in sandy form |
176 |
8 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Round |
|
|
60–65 |
| Casting |
GOST 613-79 |
in chill mold |
60 |
| Casting |
GOST 613-79 |
in sandy form |
60 |
Casting and technological parameters
Analogues
| USA |
Germany |
| C84800 |
G-CuSn2ZnPb DIN 1705 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |