BrO3Ts6S5
For the production of ingots from scrap and non-ferrous metals, used for the needs of the national economy
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Tin cast bronze |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | P, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 613-79 | < 0.4 | < 0.05 | 2–4 | 79.6–90.7 | 3–8 | < 1 | < 0.5 | < 0.05 | 3–6 | < 1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 613-79 | |
| DSTU 3474-96 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |