BrO5Ts6S5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Pewter cast bronze in pigs |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
P, % |
S, % |
| GOST 614-97 |
< 0.4 |
< 0.05 |
4.1–6 |
< 0.02 |
79.15–87.3 |
4.5–6.5 |
< 1 |
< 0.5 |
< 0.05 |
4.1–6 |
< 0.15 |
< 0.1 |
< 0.08 |
Information on suppliers
Analogues
| Germany |
USA |
| BOGRA - Rg5 |
85-5-5-5 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mg |
% |
Magnesium |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| S |
% |
Sulfur |