BrO8N4Ts2 (BrONTS8,5-4-2)
for making castings of body parts General purpose; casting parts for shipbuilding, marine-mechanical engineering.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Tin cast bronze |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
As, % |
P, % |
S, % |
|
< 0.3 |
< 0.02 |
8–9 |
< 0.02 |
82.34–87 |
1.5–3 |
3.5–5 |
< 0.02 |
< 0.05 |
< 0.15 |
< 0.05 |
< 0.05 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
Treatment |
| Alloy |
|
|
|
|
> 264.6 |
> 175 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
|
78.5 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mg |
% |
Magnesium |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |