BrOF2-0.25 (BrOF2-0,25A)
Screws, tape for flexible hoses, conductive parts, filler material for welding
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Pressure Tin Bronze |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Zn, % | Ni, % | Pb, % | P, % |
|---|---|---|---|---|---|---|---|
| GOST 5017-2006 | < 0.05 | 1–2.5 | 96.7–98.98 | < 0.3 | < 0.2 | < 0.03 | 0.02–0.3 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 5017-2006 | Wrought tin bronzes. Grades |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Pb | % | Lead |
| P | % | Phosphorus |