BrOTs10-2 (BrO10Ts2)
for the manufacture of valves, anti-friction parts, bearings, friction parts and lining propeller shafts; casting parts for shipbuilding, ship mechanical engineering.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Tin cast bronze |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | P, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 613-79 | < 0.3 | < 0.02 | 9–11 | < 0.02 | 82.59–90 | 1–3 | < 2 | < 0.3 | < 0.02 | < 0.5 | < 0.15 | < 0.05 | < 0.05 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| Germany | USA |
|---|---|
| GZ-Rg10 | Gun metal |
Standards
| Standard | Description |
|---|---|
| GOST 613-79 | |
| OST 1 90054-72 | |
| GOST 613-65 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |