BrOTs4-3
Tapes, strips, rods, used in electrical engineering, mechanical engineering; wire for springs, contacts, plug sockets, chemical equipment parts; wire for manual welding in protective gases copper mechanized submerged arc welding of copper and brass
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Pressure Tin Bronze |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Bi, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | P, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5017-2006 | < 0.05 | < 0.002 | 3.5–4 | < 0.002 | 92.2–93.8 | 2.7–3.3 | < 0.3 | < 0.002 | < 0.002 | < 0.02 | < 0.03 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$E\cdot 10^{9}$$, $$MPa$$ | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|---|---|---|
| 20 | 122 | 84 | 8800 | 0.09 | |
| 100 | 18 |
Mechanical properties at 20 °C
Brinell hardness number
Casting and technological parameters
| melting point, °C | Hot working temperature, °C | annealing temperature, °C |
|---|---|---|
| 1045 | 700–800 | 550–650 |
Analogues
| Germany |
|---|
| CuSn4Zn4 |
| 2.107 |
Standards
| Standard | Description |
|---|---|
| GOST 5017-2006 | Wrought tin bronzes. Grades |
| GOST 5017-74 | |
| GOST 1761-16 | |
| GOST 1761-92 | |
| GOST 5221-08 | |
| GOST 6511-14 | |
| DSTU GOST 5017:2007 | |
| DSTU GOST 5221:2009 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$E\cdot 10^{9}$$ | $$MPa$$ | Elastic modulus |
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter | Units of measurement | Description |
|---|---|---|
| melting point | °C | The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Hot working temperature | °C | The temperature at which the plastic-deformed metal recrystallizes during the pressure treatment |
| annealing temperature | °C | The temperature at which the processes return recrystallization and homogenization of the metal to reduce its hardness for subsequent machining |