BrOTsS4-4-2,5A
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Mg, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
P, % |
S, % |
ET, % |
| GOST 5017-2006 |
< 0.02 |
3–5 |
< 0.007 |
< 0.002 |
85.93–92.5 |
3–5 |
< 0.3 |
< 0.002 |
< 0.002 |
1.5–3.5 |
< 0.03 |
< 0.007 |
< 0.2 |