Brs
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
P, % |
Примеси, % |
| GOST 1595-90 |
< 0.5 |
< 0.1 |
< 0.1 |
1.5–2.5 |
84.56–90.5 |
< 1 |
< 0.5 |
8–9.2 |
< 0.03 |
< 0.01 |
< 1.5 |