BrSu6F1
for casting of simple shape, heavy duty
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Tinless cast bronze |
Chemical composition
| Standard |
Cu, % |
Sb, % |
P, % |
| GOST 493-79 |
91.7–94.9 |
4.7–6.2 |
0.4–0.9 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
93.1 |
|
4.6 |
8500 |
| 100 |
|
17.3 |
|
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Alloy |
|
|
|
|
216 |
5 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
|
78 |
Casting and technological parameters
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Cu |
% |
Copper |
| Sb |
% |
Antimony |
| P |
% |
Phosphorus |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| linear shrinkage |
% |
The difference between model dimensions and the model casting |