Bro.VAZHMts 10-3-1.5
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | P, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 2–4 | < 0.02 | < 0.01 | 1.3–3 | 78.58–87.7 | < 1 | < 0.5 | < 0.05 | 9–11 | < 0.1 | < 0.01 | < 0.03 | < 1.7 |
Note: GOST 17328: Upon request:Si < 0.1; P < 0.01; Zn < 0.5; All < 1.0
Note: GOST 614:Cu: Cu + Ni
Information on suppliers
Analogues
| Germany |
|---|
| CuAl9Fe3Mn2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |