BTC-VD
For the manufacture of superconducting topological generator switches in the system input and output energy of superconducting magnets; cryogenic structures.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Precision alloys superconducting |
Chemical composition
| Standard | Ti, % | Zr, % | C, % | O, % | Nb, % | N, % |
|---|---|---|---|---|---|---|
| GOST 10994-74 | 0.07–0.2 | 0.2–1 | < 0.03 | < 0.005 | 98.76–99.73 | < 0.005 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Ti | % | Titan |
| Zr | % | Zirconium |
| C | % | Carbon |
| O | % | Oxygen |
| Nb | % | Niobium |
| N | % | Nitrogen |