ChS120U-VI
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Bi, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Sb, % |
Zr, % |
Al, % |
Pb, % |
P, % |
C, % |
S, % |
Nb, % |
Y, % |
Mo, % |
N, % |
W, % |
| TU 14-134-303-92 |
< 0.35 |
< 0.15 |
0.005 |
< 5.0E-5 |
< 0.15 |
7–7.8 |
11.4–12.6 |
4–4.6 |
< 0.1 |
60.55745–66.365 |
< 0.0005 |
0.01 |
3.9–4.3 |
< 0.001 |
< 0.008 |
< 0.03 |
< 0.008 |
0.6–1 |
0.02 |
0.7–1.3 |
< 0.01 |
6–7 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Y |
% |
Yttrium |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |