CuZn35Pb2Al-C
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| DIN EN CEN/TS 13388 | < 0.3 | < 0.02 | < 0.3 | < 0.1 | 61.5–64.4 | 31.5–35.6 | < 0.2 | < 0.14 | 0.3–0.7 | 1.5–2.2 | 0.04–0.14 |
Note: For contact with drinking water: the remaining elements <0.02, the sum of the remaining elements <0.25 For applications not related to contact with drinking water it is allowed: As <0.04, Sb + As <0.14 For contact with drinking water: Sb <0.02%.
Information on suppliers
Analogues
| European Union | USA |
|---|---|
| CuZn35Pb2Al-B EN 1982:2008 | 60-40 |
Standards
| Standard | Description |
|---|---|
| DIN EN CEN/TS 13388 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |