CuZn36Pb2As
Production of fittings designed for connecting copper pipes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Brass (copper-zinc alloy) | Brass, pressure treated |
Chemical composition
| Standard | Fe, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 52922-2008 | < 0.1 | < 0.1 | < 0.1 | 61–63 | 33.5–37.08 | < 0.3 | < 0.05 | 1.7–2.8 | 0.02–0.15 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 8400 |
Standards
| Standard | Description |
|---|---|
| GOST 52922-2008 | GOST |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |