D11
Parts, products, semi-finished products and billets of non-ferrous metals and alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Ti, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | < 0.3 | < 0.3 | < 0.025 | < 0.15 | 0.9–1.3 | 97.775–99.1 | < 0.1 | < 0.05 |
Information on suppliers
Analogues
| Germany | European Union | USA |
|---|---|---|
| AlZn1 DIN 1725 Part 1 | EN AW-7072 EN 573-3:2013 | 7072 |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| OE | % | Other items |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Mn | % | Manganese |
| Ti | % | Titan |
| Zn | % | Zinc |
| Al | % | Aluminium |