D1ch
Aluminum deformable alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1 90048-90 | < 0.4 | < 0.5 | 0.4–0.8 | 0.4–0.8 | < 0.1 | 3.8–4.8 | < 0.3 | < 0.1 | 92.05–95.4 | < 0.05 | < 0.1 |
Note: Fe + Si < 0.70%
Information on suppliers
Analogues
| Germany | European Union | USA |
|---|---|---|
| AK2 | P-AlCu4MgMnSi | AlCu4MgSi |
Standards
| Standard | Description |
|---|---|
| OST 1 90048-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |