D23
Aluminum deformable alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Al, % | Li, % | Cd, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1 90048-90 | < 0.3 | < 0.3 | < 0.05 | 0.4–0.8 | < 0.15 | 4.8–5.8 | 90.75–93.8 | 0.9–1.4 | 0.1–0.25 | < 0.1 | < 0.1 |