D26
Parts, products, semi-finished products and billets of non-ferrous metals and alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | < 0.4 | < 0.4 | 0.8–1.4 | < 0.5 | 0.1–0.3 | 0.01–0.1 | < 0.1 | 4.3–5.5 | < 0.2 | 90.9–94.79 | < 0.05 | < 0.15 |
Information on suppliers
Analogues
| Russia |
|---|
| 1925С Включен в 2 стандарта |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |