D4
Parts, products, semi-finished products and billets of non-ferrous metals and alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | 0.8–1.3 | 0.5–1.2 | 1.4–1.8 | < 0.2 | < 0.1 | 1.9–2.5 | < 0.3 | 0.8–1.3 | 91.15–94.6 | < 0.05 | < 0.1 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| 2618A DIN EN 4632-002:2008 | 2618A |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |