DI-38 (90G29U9VBM)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Ca, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
W, % |
|
56.05–61.55 |
< 0.3 |
0.05–0.1 |
0.05–0.1 |
28–30 |
< 0.3 |
< 0.3 |
< 0.5 |
8.3–9.3 |
< 0.05 |
< 0.03 |
0.85–0.95 |
< 0.02 |
0.3–0.6 |
0.3–0.5 |
0.6–0.9 |
Information on suppliers
Properties
| Property |
| Calculated Properties Density: 7.32 g / cm3 |
| Note austenitic steel |
Analogues
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Ca |
% |
Calcium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |