DI-61U (10H13G18DU)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-4820-90 | 64.005–70.2 | < 0.7 | 17–18.5 | 12.5–14 | 0.3–0.6 | < 2 | < 0.045 | < 0.12 | < 0.03 |
Note: According to TU U 14-4-435-98 Cu is absent
Information on suppliers
Properties
| Property |
|---|
| Typical Characteristics Yield Strength:> 315 MPa |
| Typical Characteristics Temporary Resistance:> 640 MPa |
| Typical Characteristics Elongation:> 47% |
| Calculated Properties Density: 7.69 g / cm3 |
Standards
| Standard | Description |
|---|---|
| TU 14-1-4820-90 | |
| TU 14-226-127-92 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |