DI52-ID (03X11N8M2F-ID)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-5287-94 |
75.245–78.85 |
< 0.5 |
< 0.5 |
11–12 |
7.8–8.6 |
0.05–0.3 |
< 0.015 |
< 0.03 |
< 0.01 |
2.3–2.8 |
Information on suppliers
Properties
| Property |
| Forgings round and rectangular in accordance with TU 14-1-5287-94 Note Yield strength:> 834 MPa |
| Forgings round and rectangular according to TU 14-1-5287-94 Note Temporary resistance:> 981 MPa |
| Forgings round and rectangular according to TU 14-1-5287-94 Note Elongation:> 12% |
| Forgings round and rectangular according to TU 14-1-5287-94 Note Relative narrowing:> 55% |
| Forgings round and rectangular according to TU 14-1-5287-94 Note Impact strength KCV at 20 ° C:> 98 J / cm2 |
| Calculated Properties Density: 7.91 g / cm3 |
| Note Two-phase (duplex) stainless steel |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |