DI99-MP (R6M5F3-MP)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| GOST 28393-89 |
75.64–80.65 |
< 0.6 |
< 0.5 |
< 0.5 |
3.8–4.3 |
< 0.25 |
< 0.4 |
3.1–3.7 |
< 0.03 |
1.25–1.35 |
< 0.03 |
5.5–6 |
5.7–6.7 |
Information on suppliers
Properties
| Property |
| Products according to GOST 28393 Annealing Hardness HB: <269 |
| Products according to GOST 28393 Annealing Imprint Diameter:> 3.7 mm |
| Tempering with tempering Hardness HRC:> 65 |
| According to customer demand Hardness HB: <255 |
| According to customer requirement Imprint diameter:> 3.8 mm |
| Calculated Properties Density: 8.53 g / cm3 |
| Note Tool Powder Steel |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |