DNK-1
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Co, % | Ti, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Te, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % | Ag, % | O, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.003 | < 0.001 | < 0.0001 | < 0.0005 | < 0.0001 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.001 | < 0.0005 | > 99.92 | < 0.0001 | < 0.0001 | < 0.0005 | < 0.0001 | < 0.0005 | < 0.0001 | < 0.0005 | < 0.05 | < 0.0015 | < 0.0001 | < 0.02 | < 0.001 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Te | % | Tellurium |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Ag | % | Silver |
| O | % | Oxygen |
| N | % | Nitrogen |