E-08X20H60M15V3
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10052-75 | < 3 | < 0.8 | < 1 | 17–22 | 52.415–67 | < 0.025 | < 0.04 | < 0.02 | 13.5–16.5 | 2.5–4.2 |
Note: The chemical composition of the weld metal