E-10X25H13G2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| GOST 10052-75 | 55.33–65 | < 1 | 1–2.5 | 22.5–27 | 11.5–14 | < 0.03 | < 0.12 | < 0.02 |
Note: The chemical composition of the weld metal