E-10H25N13G2B
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Nb, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10052-75 | 54.33–64.7 | 0.4–1.2 | 1.2–2.5 | 21.5–26.5 | 11.5–14 | < 0.03 | < 0.12 | < 0.02 | 0.7–1.3 |
Note: Nb> 8 * C
Note: The chemical composition of the weld metal
Information on suppliers
Analogues
| USA |
|---|
| E309LCbT0-3 |
Standards
| Standard | Description |
|---|---|
| GOST 10052-75 |