E-15H28N10S3M2GT
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10051-75 | 50.435–61.3 | 2.5–3.5 | 1–2 | 25–30 | 0.1–0.3 | 9–11 | < 0.035 | 0.1–0.2 | < 0.03 | 1–2.5 |
Note: The chemical composition of the weld metal
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10051-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |