E-190K62X29V5S2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Co, % | Cr, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|
| GOST 10051-75 | < 7.9 | 1.5–2.6 | 50.235–66.9 | 26–32 | < 0.035 | 1.6–2.2 | < 0.03 | 4–5 |
Note: The chemical composition of the weld metal
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10051-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Co | % | Cobalt |
| Cr | % | Chrome |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |